A truss head is a lid, not a clamp
The truss head on a #10 tek screw measures about 12.5 mm across and gives near 123 square millimetres of bearing face, against roughly 95 for the hex washer head that sits on the same shank, and the first time I had that difference explained to me I assumed it was about spreading load. It is not, or at least it is not mainly, because on a steel panel there is no load to spread and the panel does not care whether you press on it with a hundred square millimetres or a hundred and twenty. The head is wider for a different reason entirely and getting that reason wrong is how a roof ends up with the right screw in the wrong place.
What the wide head does is cover a hole that is deliberately too large. On any sheet that moves more than steel does, the fastener cannot grip and let it expand at once, so the sheet gets an oversize hole, the screw clamps nothing but the washer, and the sheet slides under. The truss head is the lid over that joint, and its width is set by how far the sheet travels.
Why soft sheets need a big head and steel does not
Polycarbonate runs at about 0.065 mm per metre per degree, against 0.012 for steel, so a six metre rooflight moves roughly five times as far as the purlin it is fixed to and there is no way to clamp that difference away. Work through a forty degree swing on that six metre sheet and you get about 15.6 mm of movement at the ends, which means the hole in the sheet has to be around 15 mm for a 6.5 mm screw if the sheet is to move without tearing around the fixing. A 19 mm washer covers a 15 mm hole with two millimetres of margin and a truss head is what holds that washer flat while the sheet slides beneath it.
On a steel roof none of that applies, because panel and purlin move together and a tight hole is an advantage. So a truss head there is not wrong, it is doing a job steel never asked for, and it turns up because contractors buy one screw for the whole roof and the rooflights are part of that roof. I have seen a 3,000 square metre job specified with truss head throughout because eighty of it was polycarbonate.
The hole has to be bigger than the screw
Every failure I have been called out to on a rooflight traces back to a hole drilled at the screw diameter because the man on the gun had one drill bit and no instruction. A tight hole in polycarbonate does not hold the sheet, it converts the sheet's thermal movement into stress at the hole edge, and polycarbonate does not yield the way steel does. It crazes first, a fine network of cracks radiating from the hole that you can see if you get close, and then a crack runs and the sheet is scrap.
The number I give people is a hole 3 mm over the screw for anything up to three metres and 6 mm over past that, which is not a code figure and is a field rule that has kept me out of arguments. It is generous compared with what some panel manufacturers publish and it accounts for the fact that the man drilling is doing it off a ladder with a hand drill and the sheet is hot. A hole that is 2 mm too big costs nothing. A hole that is 1 mm too small costs a rooflight.
Where thermal movement beats clamp load
The consequence of all this is that on a rooflight the fastener is not holding the sheet down by friction, it is holding it down by the washer bearing on the sheet while the sheet floats, and that changes what you are checking at handover. What matters is not torque, because a torque figure that clamps a sliding joint is a torque figure that has stopped it sliding, and a rooflight that cannot slide will buckle in the first hot week and pull its fixings in the first cold one.
I walked a roof in Gladstone where every rooflight had a ripple between the screw lines and the contractor wanted to blame the sheet supplier. The sheets were fine. They were not the problem. Somebody had used a torque stick set for the steel panels on the same roof, and polycarbonate clamped like steel cannot expand, so it ripples. We backed forty screws off half a turn each and the ripple went away, which is not a repair I would recommend and was the fastest way to prove it that afternoon.
What the carbon steel gets you that stainless does not
Carbon steel with a zinc or zinc aluminium coating is the right default for a truss head tek screw and the reason is mechanical before it is economic. A carbon steel screw holds its hardness through the drill point and the thread, which is what lets it drill and tap in one operation without the point dulling halfway through a purlin, and coated carbon steel will do that consistently across a whole box. Stainless self drilling screws exist and they work, and the austenitic grades soften at the point in a way that shortens drill life on anything heavier than thin sheet.
Coating decides service life. Electro-galvanized at 8 to 15 microns is an interior coating. A zinc aluminium flake at 500 hours is what a coastal roof wants, and it goes on carbon steel without the hydrogen embrittlement that electroplating brings to a case hardened screw.
The failure that looks like a loose screw but is a tight one
The classic call out on a truss head installation is a screw that appears to have backed out, and the instinct is to drive it home again, which is the wrong move about eighty percent of the time. If the sheet has an oversize hole and the screw has been over-driven, the washer is compressed past recovery and the head is sitting below the sheet line, and what looks like a backed out screw is a screw that went in too far and took the washer's elasticity with it.
The tell is the washer itself. Pull one and look at the underside, and a washer that has been crushed flat with no rebound left will show a hard ring where the head pressed through the elastomer. On a rooflight that washer is now a rigid disc with no ability to follow the sheet as it moves, and the joint has become a clamp on a sliding surface, which is the one thing the whole design was trying to avoid.
What to write on the order
Say whether the screw is going into steel panel only or into a mix of steel and a translucent sheet, because that one sentence changes the head, the washer and the hole size all at once. Give the sheet length for anything translucent so the hole can be calculated rather than guessed. And name the coating by salt spray hours or grams per square metre instead of calling it galvanized, since a truss head on a coastal roof is a five hundred hour part and the man who quotes you ninety six will not mention the difference.
The head is the visible part and the part everybody thinks they understand, and it is the part that gets specified last after the shank and the length have been settled. On a steel roof that ordering works out. On a roof with a rooflight in it, the head is the reason the rooflight is still there in year five.
Hot Tags: truss head tek screws, carbon steel tek screws, tek screws for metal roofing, self drilling screws, truss head self drilling screws, metal roofing fasteners, roofing screws